BackgroundCheck.run
Search For

Peter A Klobuchar, 888222 Jackson Ave, Hammond, IN 46321

Peter Klobuchar Phones & Addresses

8222 Jackson Ave, Munster, IN 46321    219-8365856   

Hammond, IN   

8222 Jackson Ave, Munster, IN 46321    219-5884568   

Social networks

Peter A Klobuchar

Linkedin

Work

Company: N.a Position: Retired

Education

Degree: Bachelor's degree or higher

Ranks

Licence: Illinois - Active And Authorized To Practice Law Date: 1996

Industries

Internet

Mentions for Peter A Klobuchar

Career records & work history

Lawyers & Attorneys

Peter Klobuchar Photo 1

Peter M Klobuchar, Chicago IL - Lawyer

Address:
Ungaretti & Harris, LLP
Three First National Plaza 70 West Madison Street,, Chicago, IL 60602
312-9774416 (Office), 312-9774416 (Fax)
Licenses:
Illinois - Active And Authorized To Practice Law 1996
Specialties:
Intellectual Property - 34%
Litigation - 33%
Communications / Media - 33%

Peter Klobuchar resumes & CV records

Resumes

Peter Klobuchar Photo 12

Peter Klobuchar

Location:
2026 Thornwood Ave, Wilmette, IL 60091
Industry:
Internet
Work:
n.a
retired

Publications & IP owners

Us Patents

Process Of Producing One-Side Alloyed Galvanized Steel Strip

US Patent:
4171392, Oct 16, 1979
Filed:
Nov 8, 1978
Appl. No.:
5/958800
Inventors:
William C. Sievert - Chesterton IN
James B. Cundiff - La Porte IN
Peter A. Klobuchar - Munster IN
Larry H. Lindberg - Valparaiso IN
James A. Kargol - Notre Dame IN
Assignee:
Inland Steel Company - Chicago IL
International Classification:
C23C 102
US Classification:
427321
Abstract:
A process of consistently producing in an economical manner a galvanized steel strip having on one side a thin uniform surface coating of zinc-iron intermetallic compounds containing at least 6 percent iron and being free of metallic zinc and having on the other side a formable metallic zinc surface coating which is formed by continuously immersing the steel strip in a hot-dip zinc coating bath in which the temperature of the steel strip and the coating bath are controlled within a limited range to avoid forming an exclusively thick zinc iron intermetallic layer during hot-dip coating which interferes with good formability of the metallic zinc surface coating and controlling the thickness and uniformity of the zinc coating which is transformed into the coating formed of zinc-iron intermetallic compounds within a range of 10 to 30 g/m. sup. 2 while maintaining the variation in coating weight within a range of from 3 to 6 g/m. sup. 2 and heating the strip rapidly to a peak temperature of between about 482. degree. C. and 524. degree. C.

NOTICE: You may not use BackgroundCheck or the information it provides to make decisions about employment, credit, housing or any other purpose that would require Fair Credit Reporting Act (FCRA) compliance. BackgroundCheck is not a Consumer Reporting Agency (CRA) as defined by the FCRA and does not provide consumer reports.